Casting process: 1) smelting process: 1) composition: chromium, nickel alloy chromium steel.
2) tapping temperature:155015001450.
2) Cavity technology: 1) Solidification mode: not obvious, obviously obvious.
2) Molding sand: refined quartz sand refined quartz sand
3) Coating: zircon powder coating, zircon powder coating and quartz powder coating.
3) Pouring technology: 1) Pouring temperature:1480-15201450-14801420.
2) heat preservation time: medium length and short length